Butyl Reclaimed Rubber Compound Properties

Tensile Strength

Mooney Viscosity

Elasticity

Ash Content

7 MPA40-50 (100 °C,1+4)% 4906. Water 0.5
8 MPA50-60 (100 °C,1+4)% 4808. Water 0.5
10 MPA50-60 (100 °C,1+4)% 4808. Water 0.8
11 MPA60-70 (100 °C,1+4)% 46010. Water 0.8