Latex Reclaimed Rubber Compound Properties

Tensile Strength

Elongation Rate

Mooney Viscosity

Rubber Content

Ash Content

Water Content

Acetone Extraction

MPA ≥

% ≥

100°C,1 +4 ≤

%

% ≤

% ≤

% ≤

17

600

50 – 70

100

6

0.5

8

16

560

50 – 70

100

8

0.5

9

15

530

50 – 70

85

10

0.5

10

14

520

50 – 70

90

10

0.5

10

13

480

50 – 70

85

11

0.5

11

12

460

50 – 70

70

11

0.5

11

11

440

50 – 70

80

11

0.5

12

10

430

50 – 70

75

12

0.5

12

9.0

400

50 – 70

70

12

0.5

13


* For more information and specifications, please contact us